Is anyone using a TSOP48 12mm x 20mm package with the IPC SM-782 recomended dimensions? We seem to have problems with center to center measurements and also the pad size seems long and narrow. *************************************************************************** * The mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text.* *************************************************************************** * If you are having a problem with the DesignerCouncil, please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************