Lou, here is what I know about black oxide. Compunetics here has been putting black oxide on some outer layers. Solder mask adhesion was a concern. It is being used mostly for DFSM, but some LPI boards also get it. Without data to provide convincing evidence, the belief is that adhesion is better. My understanding is that at least one LPI supplier advised against black oxide. Problems in solder resist adhesion have arisen because of uneven plating across the board surface. Some regions are higher than others, so dry film doesn't always conform or the silk-screened LPI is not deposited with enough thickness. Some time back, I found a copy of IPC-SM-839. It had a lot of interesting comments on adhesion promoting treatments. I don't think black oxide was mentioned. Lou Hart 412-858-6117 . **************************************************************************** * The mail list is provided as a service by IPC using SmartList v3.05 * **************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ****************************************************************************