Maurice: Amp Inc. has a full line of SMT qualified sockets. Request catalog 65230 which includes both through-hole and surface mounts parts designed for SMT assembly temperatures. We haven't had any problem with them on our boards which are double sided mixed tech. Pam Morrison (407) 826-1424 ______________________________ Reply Separator _________________________________ Subject: ASS: Socket temperature performance Author: [log in to unmask] at ORL-SMTP-G Date: 5/14/96 7:48 AM In a wave soldering process a plastic socket on the underneath has to be soldered on afterwards following the process. Are there any high temperature plastic sockets available which can go through the Wave Soldering process. Appreciate any comments, information, suggestions. Thanks in advance.