When we were in the board fabrication business, we did not store layers in a vacuum with desiccant but when we used vacuum frame we would pull a vacuum and hold it for more than 30 minutes before lamination. When we switched to a vacuum lamination we continued to use a vacuum in the press and hold before lamination. We also pulled a vacuum on the prepreg and back filled it's storage chamber with dry nitrogen. The froth at the edge of the board when down but we did not know if that was from the vacuum steps or the fact we went to low pressure lamination when we switched to vacuum lamination. ---------- From: [log in to unmask] To: [log in to unmask] Subject: Vacuum Desiccating Date: Friday, August 30, 1996 6:38AM Has anyone done testing, or incorporated as part of normal processing, the use of vacuum desiccating instead of baking after layer oxide coating, prior to lay-up and lamination. I would appreciate any information that is available. Bob G. *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************