John: I started my illustrious circuit board career 20 years ago in the drill room. At that time, obviously we weren't dealing with .010" drills in BUT boards (big, ugly, thick). We did, however, have our share of broken drills. Because carbide is hard but brittle, we used to use tools that were like an elongated pushpin to push the drill bit residue out of the hole. I would assume that the same could be used nowadays, just smaller. Maybe a needle would work. It would have to be something which is a hard metal. Also, unless the board has multiple parts per panel, oftentimes the hole is damaged, looking more like an egg than a circle. It usually causes scrap. Good luck! Tom Coyle Field Services Engineer HADCO Corporation *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************