There are two schools of thought on the effect matte surface finish has on solderballs. 1. The matte surface typically has a lower surface tension, allowing better wetting of no-clean flux to the mask surface. The no-clean flux forms an insulation barrier, preventing solder from sticking to the mask. 2. Because of the irregular surface, typically produced by a matte solder mask, there is less surface area for solder balls to adhere to. Your second question requires input from your solder mask vendor. Your solder mask vendor should have a list of compatible conformal coatings. Bob Metcalf Morton Electronic Materials >>> JIM ENNIS <[log in to unmask]> 08/20/96 08:27am >>> We are beginning to see more PCB suppliers offering matte finish LPI. We have heard that this finish reduces the adherence of solderballs. Is this true? If so, at which process, reflow or wave? What is the science behind this lessening of solderballs? 2nd Question: We are also starting a project that will require conformal coating. Is there a preference in solder mask type/finish? The coatings we are leaning towards are silicone-based. *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************