From: NAME: WILLIAM G KENYON FUNC: Chemicals/Electronics TEL: 302-652-4272 <KENYONWG AT A1 AT ESVAX> To: NAME: [log in to unmask] <"[log in to unmask]"@ESDS01@MRGATE@ESVAX> Suggest you contact Branson or Crest for a small table-top unit, probably with ultrasonics. If you are doing both rosin and water soluble in same unit, might look into the inorganic saponifier, since will do both and not a VOC issue, since you will have it in the work area as opposed to in area with exhaust hood, where there are other water soluble organic options. The alkaline saponifier will tend to kill the active water soluble residues, so should help minimize potential microetching of the solder joints from the water soluble flux.