Could you possibly be talking about the organic surface protectant ENTEK? If so contact Enthone-OMI at 203-934-8661 or email [log in to unmask] These coatings are widely use in surface mount component applications because they give flatter surfaces for solder attachment of the parts than hot air solder leveling ---------- From: [log in to unmask] To: [log in to unmask] Subject: Entech Date: Tuesday, August 06, 1996 2:34PM One of our students is looking for information on the Entech coating process for copper lines. Can anyone tell me where to find that? I have heard of it as a process ... is it a company as well? Ron Gedney [log in to unmask] Integrated Electronic Eng. Center Watson School of Eng. & Applied Science Binghamton University P.O. Box 6000 Binghamton, NY 13902 607-777-4335, fax 4683 *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************