We are experiencing a small but troublesome fallout from crushed pins on a PCI type connector. The connector supplier said that the nickel is the cause. The logic is that the nickel wears slower than the copper or gold and therefore tends to protrude and form a 'hook' that will snag and crush the pins. The nickel may also not be beveled properly because of its hardness. The proposed test is to create a PCB out of steel with a number of bevel angles and 'hooks' and insert into connectors. My understanding is that nickel is harder than steel, but does this test sound logical? *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************