Nora and Dave, Here is a message from a colleague of mine about Menisograph Solderability Testers. Tom Carroll Hughes Aircraft Co. (310) 334-4757 _______________________________________________________________________________ Subject: Re[2]: ...no subject... From: Richard T Lamoureux at 3-DUCKS Date: 7/11/96 8:41 AM Tom, I don't know how to gert this to techNet so please pass it on. Nora, I have S/N 196 which is on the border of when a significant change was made about 1987. If you have any specific questions please feel free to contact me at Hughes Aircraft Co. 310-616-6174. ps: Dave got the rep right but I don't believe he got the age of his machine right. They weren't making the MK VI in '68, maybe '86. Dick Lamoureux ______________________________ Reply Separator _________________________________ Subject: Re: ...no subject... Author: Thomas A Carroll at 4-SDCCM2 Date: 6/3/96 11:50 AM Richard, I thought you would be interested in these messages. I do not know the age of your machine, but I thought that you could possibly help Nora with some information and that you could use these contacts for future work. Reply to these individuals using their internet e-mail addresses. Tom _______________________________________________________________________________ Subject: Re: ...no subject... From: [log in to unmask] at CCGATE Date: 5/24/96 6:22 AM Good morning TechNet! Nora - try: Dage Precision Industries 46701 Fremont Blvd Fremont CA 94538 510-683-3930 510-683-3935 fax I have a 1968 GEC Mark VI Meniscograph that is running like the Everready Bunny - anyone have one that is older? Dave Hillman Rockwell Collins [log in to unmask] ______________________________ Reply Separator _________________________________ Subject: ...no subject... Author: [log in to unmask] at ccmgw1 Date: 5/23/96 6:11 PM Hi - I am looking information on GEC meniscograph tester. Does anyone has any information on this tester? Nora Xiao [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************