You are going to have trouble meeting all of the visual requirements with hot bar attach. It is a side effect of the attach method. I had to have special visual requirements for it, and these were not in any standard. Maybe there is something now. I do not know. ______________________________ Reply Separator _________________________________ Subject: FWD>assy: hot bar solder jo Author: [log in to unmask] at internet Date: 7/10/96 7:40 PM this message is being forwarded from a co-worker, the solder joints that we are forming with our hot bar process are not meeting the requirements of 'standard' workmanship criteria. in particular, we have a difficult time meeting 'heel fillet' requirements. the defect is one of 'insufficient solder' at the heel fillet. it isn't that there isn't any heel fillet; it's just that it isn't as pronounced as the standards require. question.- are there solder joint standards specific to hot bar soldering? thanks, phil crepeau, trw-san diego Judy Murray TRW San Diego 619.592.3616 [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************