We are using a material called "Matrix Moe" supplied by: Elastomeric Technology Inc.in Hatboro, PA phone 215-672-0787 fax 215-672-4633 The material consists of oriented gold conductors which are approximately 13 microns by 125 microns. The conductors are embedded in a silicone elastomer matrix. _______________________________________________________________________________ Subject: FAB; ASSY: Conductive Elastomer From: [log in to unmask] at Internet Date: 7/8/96 6:13 PM Hello TechNet... Has anyone ever seen a conductive and machinable elastomer? If so please let me know a sorce that I can contact. We need such a material for electrical testing of wirebond pads at a pitch of 175-225 microns. Any suggestions and tips are welcomed. Best Regards, Mike Freda ProLinx Labs 408-227-0707 x105 408-227-6529 (fax) The mail list is provided by IPC using SmartList v3.05 To unsubscribe from this list at any time, send a message to: [log in to unmask] with <subject: unsubscribe> and no text. The mail list is provided by IPC using SmartList v3.05 To unsubscribe from this list at any time, send a message to: [log in to unmask] with <subject: unsubscribe> and no text.