Just a caution. Many solderpaste actually recommend or even require a prebake prior to reflow. Note that an N2 atmosphere prevents oxidation of the PWB, the pastes (and fluxes) are formulated to tolerate (and even benefit from) some pre-baking (to activate the flux and drive off solvents) and prebaking also acts to reduce thermal shock during reflow. Jim Maguire Boeing [log in to unmask] ______________________________ Reply Separator _________________________________ Subject: Re: ASSY: Baking before wave soldering Author: [log in to unmask] at esdigate Date: 6/19/96 5:59 AM Teik, I'm not sure about the baking of inserted boards before wave soldering, but I do know that baking a board that has solder paste on it prior to reflow is not a good practice to start. If you are using an extremely good paste and conditions are ideal, you might get away with it, but even then you would be lucky. When you bake solder paste, you are oxidizing the board, component leads and the solder balls in the paste. Now flux is active to some degree at room temperature, and that activity increases with temperature. How much the activity increases depends on the flux formulation. So here you have you solder surfaces oxidizing and your flux becoming more active (trying to remove all of this oxidation) and before long your flux puts up a white flag because there is more oxidation than it can remove. Now you have an oxidized board with an exhausted flux going into your reflow oven. Your board will have less that good results. If you feel you really need to do this, I would get some test boards and dummy components. Use these to develop a bake cycle that works with the flux and board conditions you have to deal with. Best of luck. > A customer of ours is asking what is the best practice baking > procedure (or pre-conditioning) of loaded board prior to IR reflow or > wave soldering. > > All of our specs in house deal with bare boards. I know there must be > an IPC assy spec that specifies boards pre-conditioning at reflow. Can > someone tell me the spec#, temperature and duration? > > Thanks. > > Teik M. Ng > [log in to unmask] > PC World > Toronto, Canada > > Sincerely, John Guy EMPF tel: (317) 226-5630 fax: (317) 226-5615 E-Mail: [log in to unmask]