Please send a more detailed description of the "splashes" - where are they on the assembly, what they look like, etc. Dave Hillman Rockwell Collins [log in to unmask] ______________________________ Reply Separator _________________________________ Subject: PCB Assy-Wave Solder Author: [log in to unmask] at ccmgw1 Date: 6/17/96 11:37 AM Presently we are seeing accurrances of solder splashes in our wave solder process. We have PCB's that are less then three months old and our storage process is inside of a ziplock bag with desiccant. Our present environment has a higher than normal humidity level of 40 to 50%. We have attempted many adjustments to the proces such as speed, flux gravity(foamer), etc.. The only thing that appears to eliminate or reduce the splashes is baking the assembly for 1 hour at 50 degrees 'C' and doing the wave process while the assembly is still hot. Does anyone out there have any ideas of what could cause this problem or things we should try that could eliminate them? Thanks in advance