Jeff, Do you have any vibration requirements? If the gold is soft it could wear out prematurely if vibration levels cause movement of the connection. Tom Carroll Hughes Aircraft Co. [log in to unmask] _______________________________________________________________________________ Subject: gold plating From: [log in to unmask] at CCGATE Date: 6/12/96 11:04 AM I have designs with gold plated contact areas on microwave stripline circuits. The contact area is used to make a pressure connection between the circuit and an RF connector. The connection is made by compressible gold mesh (super miniature brillo pad) placed in the space between the circuit contact area and the center pin of the RF connector. The drawing currently specifies gold plating per Mil-G-45204, Type II, Grade C, Class 1. Our supplier has requested that they be allowed to use Grade A (softer) gold instead. IPC-D-275 does not recommend Grade A for contact areas but I think this is based on a wiping action across the surface when the connection is made or broken (eg. connector fingers) and the soft gold would not provide adequate wear resistance. Our design has the contact area under continous compression. Anyone have any experience which would indicate the Grade A gold would be a poorchoice in this application? Thanks for your help. Jeff Rowe Lockheed Martin Syracuse, NY [log in to unmask] The following is an attached File item from cc:Mail. It contains information that had to be encoded to ensure successful transmission through various mail systems. To decode the file use the UUDECODE program. --------------------------------- Cut Here --------------------------------- begin 644 rfc822.txt M1G)O;2!496-H3F5T+7)E<75E<W1`:7!C+F]R9PT*6"U%;G9E;&]P92U&<F]M M.B!496-H3F5T+7)E<75E<W1`:7!C+F]R9PT*4F5C96EV960Z(&9R;VT@<VEM M;VXN:7!C+F]R9R`H,38X+C$Q,RXR-"XV-"D-"B!B>2!%1$5.+DA!0RY#3TT@ M*%!-1$8@5C0N,RTW(",U.#@T*2!I9"`\,#%)-51(5#)3-T-7,#`Q2S@S0$5$ M14XN2$%#+D-/33X[(%=E9"P-"B`Q,B!*=6X@,3DY-B`Q,3HP-#HP.2!04U0- M"E)E8V5I=F5D.B!F<F]M(&EP8RYO<F<@8GD@<VEM;VXN:7!C+F]R9R!V:6$@ M4TU44"`H.30P.#$V+E-'22XX+C8N.2\Y-#`T,#8N4T=)*0T*(&ED($U!03$R M,CDQ.R!7960L(#$R($IU;B`Q.3DV(#$R.C4X.C(W("TP-S`P#0I296-E:79E M9#H@8GD@:7!C+F]R9R`H4VUA:6PS+C$N,C@N,2`C,BD@:60@;3!U5'4U<RTP M,#`P1$A#.R!7960L#0H@,3(@2G5N(#DV(#$R.C4R($-$5`T*4F5S96YT+61A M=&4Z(%=E9"P@,3(@2G5N(#$Y.38@,3(Z-3@Z,C<@+3`W,#`-"D1A=&4Z(%=E M9"P@,3(@2G5N(#$Y.38@,3`Z,3<Z-#D@+3`T,#`@*$5$5"D-"E)E<V5N="UF M<F]M.B!496-H3F5T0&EP8RYO<F<-"D9R;VTZ(')O=V5`<WER+F=E+F-O;0T* M4W5B:F5C=#H@9V]L9"!P;&%T:6YG#0I297-E;G0M<V5N9&5R.B!496-H3F5T M+7)E<75E<W1`:7!C+F]R9PT*4F5S96YT+7-E;F1E<CH@5&5C:$YE="UR97%U M97-T0&EP8RYO<F<-"E1O.B!T96-H;F5T0&EP8RYO<F<-"E)E<V5N="UM97-S M86=E+6ED.B`\(DIT>4),,RXP+E]T1RY:1FUL;B)`:7!C/@T*365S<V%G92UI M9#H@/#DV,#8Q,C$T,3<N04$P,#4W-D!E-7-B830V/@T*0V]N=&5N="UT<F%N M<V9E<BUE;F-O9&EN9SH@-T))5`T*3VQD+5)E='5R;BU0871H.B`\<F]W94!S M>7(N9V4N8V]M/@T*6"U-86EL:6YG+4QI<W0Z(#Q496-H3F5T0&EP8RYO<F<^ M(&%R8VAI=F4O;&%T97-T+S0V-#D-"E@M3&]O<#H@5&5C:$YE=$!I<&,N;W)G 4#0I0<F5C961E;F-E.B!L:7-T#0H` end