One of the standard tests for Copper cleanliness is simply to drop some standard 0.1N Silver Nitrate titating solution on to the Copper. If the Copper is clean, the Silver Nitrate turns black almost immediately. If there are soils present, the copper remains pink/orange. Is this what you were referring to?? Rudy Sedlak RD Chemical Company