The formation of a corrosion product wit tin-lead/gold requires some environmental condition such as moisture or perhaps oxygen. I have examine solder plug-ins to gold connectors after 3 years and saw no signs of fretting or corrosion; however, the environment was dry and kept dry. In other cases the environmet was dry nitrogen and the connections looked exactly like they they did when they were connected. Phil Hinton [log in to unmask]