You can get the foils from several vendors: AlliedSignal, ADI/Isola, et.al. If you are using it as a stand alone item (no prepreg), the only thing you should really be concerned about is the amount of resin that is actually available to fill around the circuits. Normal resin coated foil has about a 1.5 mils of resin. This is a universal process limitation from all the vendors. I recommend that you get it double coated with resin. They apply a first layer of resin which is C-staged to about 7/10 mil thick and then coated again with resin. The second coat is b-staged. This will assure you of at least a minimum dielectric separation. The biggest problem we had was getting fill around all of the circuits. You will need to use a conformal film of some type, i.e. tedlar. Keep in mind that after you do this you'll have A LOT of image transfer. ______________________________ Reply Separator _________________________________ Subject: FAB: Resin Coated Cu - Tech Ques's & Availability Author: [log in to unmask] at corp Date: 5/20/96 9:56 AM Does anyone have names and numbers for people/companies who I could contact in regard to: 1. Technical questions related to resin coated copper foil. 2. Availability - Companies that sell resin coated copper foil. Thanks, Adam Davies [log in to unmask] Voice Mail - 603 329-4000, Ext *108