Mark, Our immediate response is: You have a problem. 1) There would always be a concern in allowing vias to "plate shut". a. Were any plating chemicals trapped within the hole as it was plated shut? Probably These could react with the hole wall since they are acidic and acids dissolve plated copper. b. Is the hole completely plated shut or is there a small orifice which will allow other chemicals and cleaning products to be trapped within and react similarly as plating chemistries? c. Why in the world would a board mfg need to plate 13 mil vias in a 93 mil or 62 mil thick board closed. It would take 7.5 mils of plating at the knees to close these holes. That is not satisfactory plating. Plating 1 mil of copper in 13 mil holes in these thicknesses/aspect ratio boards is not uncommon. Plating them shut leads to all sorts of questions regarding the plating on the rest of the board. a. If the holes are plated shut, it is most likely that there is very little plating in the centers of the holes. How thick is it? b. There could be voids (not circumferential) and thin copper in the barrels which would pass continuity testing, however could crack during assembly. c. If this is the case - all holes are suspect. 3. Opens in any plated through hole can be caused by 1. Absence of copper plating due to voids or cracks. These are both directly related to plating. A break down of the etch resist can also lead to voids. 4. Electrical tests would detect complete circumferential break in hole wall plating, however it will not detect plating conditions which degrade as a result of assembly operation. 5. You should be concerned about the via and plated through component hole integrity of all board supplied since it appears that you have a degrading product. How do you proceed? 1. You must determine the exact failure mechanism. This is going to have to be done with microsections to determine why the via has failed. In addition component holes must be microsectioned to determine if they have the same condition which could degrade during the life of the board. 2. Did you buy these boards to an IPC spec, or an inhouse spec? Did you require any testing of the boards by the board mfg prior to their being shipped to you? If so you need to review their microsection data. Susan Mansilla ROBISAN LABORATORY 317-353-6249 317-357-1270 fax