Subject: Re: Repair of PCBs Bill, You will find a section on Substrate Repair under IPC-R-700 Section IV procedure 4.1.1.4 I have done repairs of this sort based on this method. After The Epoxy touch-up Material is baked with fiberglass tape around it. We would remove the tape and take a file and file the cured epoxy touch-up flush with the board to make it dimensionally correct. Good Luck Nancy Nelson DELL Computer Corp. ______________________________ Reply Separator _________________________________ Subject: Repair of PCBs Author: [log in to unmask] at Dell_UNIX Date: 1/23/96 1:53 PM I have an infrequent situation where a PCB is dropped and the corner is damaged. Is there a defined process or any training available on conducting these types of repairs? I would rather not contract out the repair work. Bill Barthel Electronic Assembly Corp. [log in to unmask] (414) 751-3651