Wait a minute. Are you vacuum sealing into one of the corrugated backed stacks with all the little holes punched in it. Or are you vacuum drawing a bag (with desiccant inside) and heat sealing the open end of the bag. The latter way, at least so I've been told, can induce corrosive gases that can actually impair the shelf life. (From the heat sealing operation.) Now I haven't actually seen this but many military accounts that I serviced stated this in harmony. DHH ______________________________ Reply Separator _________________________________ Subject: re:ASSY: Moisture sensitivity? Author: [log in to unmask] at SMTPLINK-HADCO Date: 5/5/96 9:39 PM We request PCB suppliers to do a final baking before vaccume seal PCBs in a pack of 20 (board size of 6" x 4") with a desiccant pack before shipment. Suppliers mark the date of baking on cartons for receiving and internal usage control. We only re-bake the PCBs if date of use is > 3 months from date of baking. PCBs are stored in original carton boxs (sealed) until go to Pick & Place machine and this helps to slow down the moisture absortion. regards. ----------------------[Reply - Original Message]---------------------- Sent by:"Dill, Norm J" <[log in to unmask]> Our air conditioning system here mixes in a large volumes of outside air to help control the inside temperature while economizing on energy costs. As a result, the inside and outside humidity levels are very similar. Our PWB s (FR4 & polyimide) are purchased and stored with desiccant included in each package of 10. At best, this results in slightly higher costs from our suppliers, extra handling in our stock room and later baking steps. We are considering restructuring our PWB stocking procedures. Does anyone have pro/con examples of board storage in this kind of environment? For example, does the desiccant actually keep the boards from absorbing moisture during high humidity days? What would be expected if the boards were wrapped/stored in slip sheets and bound with duct tape or left open on the shelf? If the humidity was controlled, could the desiccant and some baking steps be eliminated without an increase in warpage problems. Any opinions, examples or references will be appreciated. Norm Dill [log in to unmask] =====================================================================