Thad, guide line to specify conductor to PCB edge spacing are: minimum standard Internal layer 0.020 inches + process variation 0.050 inches+ process var. External Layer 0.100 inches + process variation The purpose being not to expose the conductor to the environment that may cause corrosion or migration. Pratap Singh RAMP Labs