-- [ From: michael carano * EMC.Ver #2.10P ] -- If your electroless copper is of sufficient thickness and you employ a microetch that will give you consistant and predictable etch rates, you should not experience any problems. But, the key here is really the consistency of the microetch. With respect to the electroless copper deposit, my experience has shown that a fine tight grained elctroless deposit will give more consistant and predictable etch rates than a porous deposit of equal thickness.