We have found that when using LPI soldermasks the undercut can be minimized by using clear or unpigmented soldermask! All vendors can supply the Fab house with this soldermask color. Also in the latest revision of the IPC-SM-840 (C) approves using clear or unpigmented soldermask. ______________________________ Reply Separator _________________________________ Subject: Re: PCB Build - dendritic growth Author: [log in to unmask] at corp Date: 4/23/96 5:17 AM Stephen, The only time I have seen this problem was when the soldermask om the board had undercut around pads. The undercut trapped contaminates. We defined the defect as typeI and typeII. TypeI : This type of soldermask undercut leaves a small path under the mask to a feature such as a pad. TypeII : This type of soldermask undercut leaves a large path to a feature. The typeI is more serious in that it trapes more contaminates. This pcb ran 10vdc @ 0.010' spacing and under humid conditions. We scrapped the boards. --------------------------- John Laur (PCB Design) Rockwell Automation Allen-Bradley Co Inc. 1201 South Second Street Milwaukee, WI 53204 +1 414 382 2162 (fax) +1 414 382 2393 (phone) [log in to unmask] --------------------------- > From [log in to unmask] Mon Apr 22 15:38:59 1996 > Resent-Date: Mon, 22 Apr 1996 15:28:09 -0700 > Resent-Sender: [log in to unmask] > Old-Return-Path: <[log in to unmask]> > From: [log in to unmask] > To: [log in to unmask] > Subject: PCB Build > Resent-Message-Id: <"DuC9E1.0.MeB.Of-Un"@ipc> > Resent-From: [log in to unmask] > X-Mailing-List: <[log in to unmask]> archive/latest/3574 > X-Loop: [log in to unmask] > Precedence: list > Resent-Sender: [log in to unmask] > Content-Length: 487 > X-Lines: 16 > > From: Stephen Ayotte > \\\\\\\EM Quality Engineering > \\\\\\\Bldg. 14-3 Col F5 5-1537 > Subject: PCB Build > Does anyone have any experience with the spacing between > PTH lands and a power plane on the external to avoid/prevent > dendritic growth between the PTH and the power plane? > > The power plane is going to have 48 volts of applied bias. > The PTH could be ground or some other signal applied bias. > > Thanks. > > **** IBM MD Product Quality Engineer**** > **** OEM Quality Engineer **** > >