Is anyone using components (such as TSOP,etc.) that have alloy 42 leads on thin card PCMCIA's? I have heard that reliability may be an issue (less compliancy) due to handling/assembly/encasement flexure. Solder joint cracking is said to be evident in reliability testing... Thanks marko