Pablo: I can't tell you what the IPC prefered pad size is, but I can tell you what we use: Three pads, each = 0.050" wide by 0.065" long \\'''''// (o o) @----oOO---------(_)----------------@ | Harry O'Halloran | | [log in to unmask] | | DSC Communications Corporation | | MS 323 | | 1000 Coit Rd. | | Plano, TX 75075-5813 | | (214) 519-3916 | @--------------------------oOO------@ |___|___| | | | | ooO Ooo ______________________________ Reply Separator _________________________________ Subject: Pad size on SOT23 Author: [log in to unmask] at SMTPLINK Date: 1/18/96 1:53 PM Pablo Mesa The Morey Corporation [log in to unmask] Can anyone tell me the IPC prefered pad size for bottom side SOT23 packages?