Good day to all, Can some of you tell me how you ship (packaging) your FULL size panels after surface finishing (plating), or how you receive them in order to avoid any damage to that finish? We currently use rigid plastic cases with sulfur free paper in between every board. We have seen, in some instances, some scratches and some contamination of the boards (the gold being so soft). Is anybody offering some type of off the shelf packaging that could offer full protection of the plating on the surface of the board? I have seen some packaging where the boards were held up-right by the edges and where there was no contact with the sides of the panels, but not for FULL size and semi-rigid boards. Thank you for any ideas/comments! Denis Dionne, Eng., M.A.Sc. [log in to unmask] Plating services, Bromont plant IBM Canada Ltd (514) 534-6724