Todd: This customer of yours is probably referencing old Military Soldering Standards such as WS6536 or Mil-S-45743 where these kind of rules existed. I can't reference the specific paragraphs for you because the copies of my specs are either long gone or packed away in storage. My question to you would be, "What specifications have been imposed on the program that you are working on ?" If you are working on military hardware with these old specs imposed, your customer may be right. The old specs were very specific as to the difference between repair and rework. Reworks were permitted with minimal recording of data but repairs seemingly required congressional approval before work could be done. If it were me I'd check and see where your customer is getting his requirements from. Bill Kasprzak Moog Inc. [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************