We have evaluated this finish and found it works well with good bonding, and no pink ring in evidence after processing. The finish is a reddish brown which appears dark brown after bonding and is similar to black oxide once solder mask is applied. The chief benefit is that it can be used in horizontal conveyorised equipment. Vertical application is not recommended although possible. The cost is claimed to be lower than reduced black oxide and the process more easily controlled. In your message dated Thursday 19, December 1996 you wrote : > > Our company is thinking about testing the Alpha preq process from alpha > metal to replace our black oxide process. Unfortunately, not many people > have experience about this process in this part of world. We will appreciate > if anyone got some comments for that. Thanks in advance! > -- Paul Gould EMail [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************