A couple of questions, 1. Are you using the turbulent wave with the lambda wave? The added thermal transfer that the turbulent wave will add to the card may help improve your solder filling problem. 2. What temperature is the topside of the board at before contact with the solder wave(s)? Going somewhat hotter then your flux manufacturers recommended temperatures in not always a bad thing. I would think it would be better to run hotter and get some solder up in the barrel then to run cooler and not have solder fill. As long as components are not being damaged. 3. What type of fluxing application are you using? foam/spray Foam may give you a little more flux up into the barrels. ---------- From: TechNet-request To: Technet Subject: ASSM: Top fillet formation Date: Friday, December 20, 1996 06:34 Hello Technetters, I need some advises. I have a 6- layers board. I try to wave solder it, the solder at the ground point is not able to flow up to the top side of the board, in fact, it doesn't flow above 75%. We have tried using a solder-iron and set to temperature to 450 deg. cel. and hopefully able to force the solder through the PTH. Too bad, it didn't work anyway and it in fact has caused some lifted pads. We use full blow Nitrogeneous wave-solder machine, and the flux we use is only 1.2% solid content. And if the preheat temperature set to high, the flux gets degraded before it even reaches the wave.. I would like to know if anyone could advise me how wave-solder such a board with a great heavy thermal mass. Thanks in Advance.. =-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-==-=-=-=-=-=-=-=-=-=-==-=-=-=-=. / Kong Hui Poh / / Techgate / / - The Technological Gateway - / / Email Add: [log in to unmask] / / / / Fax Number: (65) 842 0318 / / ............................................................................ ................................../ /_________________________________________________________________/ *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************