Mike: Solder will oxidize as it sits exposed to air. I heard someone give a talk about a non-destructive test that can be done called SERA (Sequential Electrochemical Reduction of oxides Analysis). This can be used to determine solderability. His name was Peter Brattin with ECI. Address is [log in to unmask] I hope this helps. D. Chew