All component suppliers specify a recommended reflow profile. Start from there and see what works with your process within the window. ______________________________ Reply Separator _________________________________ Subject: Peak Soldering Temp. Author: [log in to unmask] at internet Date: 12/12/96 7:47 PM Hi, I am fairly new to the PCB industry. But when I read the book about the reflow soldering process, it takes normally 213C as the peak soldering temp when the melting point of the solder may be, say 183C. My understanding is that, it takes sometime to melt and acheive a good solder joint. But how to determine 213C? Or put it this way, what is the minimum peak temp. one should maintain? Have you come across any literatures that talk about it ? Any input is appreciated. Thanks. Y.F. Wong *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************