In your message dated Tuesday 10, December 1996 you wrote : > We currently use conventional green soldermask on our doublesided FR-4 > boards. For a special application, we need the top of the board to be mostly > white. Is there a white soldermask available? We make our own boards. I believe Coates have a range of colours including white, red, blue, and black available in XZ15 which is a two pack epoxy for screen print application. If you do not have a contact address then email me direct. An alternative might be to use a white 2-pack epoxy notation ink as it is only the top side that you need it for. -- Paul Gould EMail [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************