Whoops! Terry: What I meant to say was "Any chemical found in NORMAL PCB processing will not attack polypropylene, at normal processing temperatures. Ahh, yes, somewhat different. And of course all the chemicals that you listed are not normally found in pcb processing, although there are those that say that some use of Vaseline is common in the industry ......but that is another story......;-) Thank you for the "heads up" Rudy Sedlak RD Chemical *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************