I agree! BUT in my day job we have all LPI masked boards SMOBC, HASL and tent vias. We are high volume, low cost consumer stuff and have seen no reliability issues to date. We tent both sides of 25 mil vias and see both reflow improvement (vias closer to lands) and acceptable wave (we try to keep vias out from under ICs). I cannot disagree with all the Doubting Thomas types but it do seem to work for us. I would recommend a low volume build to test your processes before switching over with any of your designs (just in case your application does not fit). There really are lots of variables, so check closely to make sure you don't get burned!!! FNKEC *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************