Date : 23/11/96 16:56 Msg From: PROCESS ENGINEERING hello, we are facing a problem of spreading of paste flux (water soluble paste) on either side of the pad just after printing (contact printing using 6 mil laser cut stencil). This is clearly observed under 4x magnification, particularly for 20 mil pitch component. is there any flux spread test for solder paste . regards nalin altos india ltd. altos india ltd. *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************