Hi! The report everyone is looking for is: "Evaluation of Low Residue Soldering for Military and Commercial Applications: A Report from the Low-Residue Soldering Task Force", June 1995 contact: Ron Iman, Sandia National Labs, [log in to unmask] Dave Hillman Rockwell Collins [log in to unmask] ______________________________ Reply Separator _________________________________ Subject: Re[2]: No clean and RF Author: [log in to unmask] at ccmgw1 Date: 11/22/96 3:05 PM Thanks for all the data. i do not remember how I got the report. Do they have it it at EMPF? ______________________________ Reply Separator _________________________________ Subject: Re: No clean and RF Author: [log in to unmask] at Internet Date: 11/22/96 2:04 PM We have been using no-clean on a number of RF boards that are made of a number of materials from FR4 to duroid and have experienced no ill effects. In fact we had more problems from the cleaning materials when using an RMA solder and cleaning the flux off the board and out of the assemblies. I also would like to know how to get a copy of the CRADA report you mentioned in your inquiry. ______________________________ Reply Separator _________________________________ Subject: No clean and RF Author: [log in to unmask] at _internetcc Date: 11/22/96 9:04 AM Anyone have any experience with no-clean residues and RF performance. I have already seen the CRADA report, which reported no problem. *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************