Harlan: More contacts: Von Roll Isola, USA PO Box 259 North Clarendon, VT 05759 USA 1-800-65-ISOLA 1-800-654-7652 Outside USA or Canada 802-775-4220 Telefax 802-776-2261 Harlan: Composite Delmat material is produced by Von Roll Isola, Delle France. Tel.:84 36 84 36 Fax. 84 56 26 27 There are several sources of Delmat in the US, two that I know, are. MB Manufacturing Rockaway, NJ. Tel.: (201) 586-2988 Fax.:(201) 586-1692 Stone Mountain Tool Conyers, Georgia Tel.:(404) 929--0166 or 1-800-624-TOOL Fax.:(404) 929-0226 ______________________________ Reply Separator _________________________________ Subject: FAB: DELMAT Author: [log in to unmask] at Internet Date: 10/31/96 2:08 PM I've got an easy question.....I hope. Does anyone have the phone number and/or E-Mail address for the Manufacturers of "Delmat"? I believe it is a French Company called "Von Roll" but I may be wrong. Harlan [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************