Hi Dan. Zero....if the MLB / Material is fully cured coming out of the press. Run Tg's. Groovy ______________________________ Reply Separator _________________________________ Subject: FAB: Post-Lam Bake Author: [log in to unmask] at SMTPLINK-HADCO Date: 10/30/96 6:39 PM What is a typical cycle for baking FR4, rigid, multilayers after lamination? Why is this bake necessary? Any information would be greatly appreciated. *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************