The companion computer program for a paper we presented (Analysis of Flex Circuit Physical Characteristics) last week at Flexcon '96 is now available on our homepage: http://www.rogers-corp.com/cmu It provides a simple way to do comparative analysis of various flex circuit constructions for: Stress/Strain Relationships Positioning the Neutral Axis Determining the Moment of Inertia and Bias Forces Heat Flow Properties Thermal/Hygroscopic X-Y & Z Axis Expansion Estimates Andy Magee - Applications Engineer Rogers - Circuit Materials Tel: (602) 917-5237 Fax: (602) 917-5256 E-mail: [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************