We use large quantities of pin and screw terminals from multiple suppliers and a burn-off flux. Periodically, we returned terminals to a specific supplier for solderability issues (which OA flux did not totally resolve). We haven't needed to do this for a couple of years. We almost never have problems with terminals within a connector. Work with your suppliers on improving incoming materials and solderability problems will be resolved. ______________________________ Reply Separator _________________________________ Subject: Re: Terminal Solderability Author: [log in to unmask] at internet Date: 10/17/96 8:18 PM Hi Ed- There are not any major changes in store for terminal solderability testing in the ANSIJ-STD-002 (components) specification (unless the committee gets a suggestion to change something). However, there will be some serious discussions in the 002/003 solderability committees on the use of"R" flux versus some activated flux (an RMA) or a low residue type flux for solderability testing. More info should be available after the Naples IPC meeting. My experience with low residue or no clean type fluxes (there is a difference) is that the amount and type of activators used are much less aggressive, quicker to "burn" off, and more soldering technique sensitive. After a short learning curve period we have had very good success with using low residue fluxes in manufacturing. Your terminal finish alloy is a high Sn finish - tin preferentially oxidizes and thus the higher the tin content the faster solderability will be impacted. Also bright acid tin finishes tend to have more solderability problems because of codeposition of the plating bath brighteners if not controled closely. A 320 microinch thick finish should be enough to maintain solderability unless the storage conditions are really bad. You might try switching to a lower tin content alloy if your design permits it or maybe some pretinning. Good luck. Dave Hillman Rockwell Collins [log in to unmask] ______________________________ Reply Separator _________________________________ Subject: Terminal Solderability Author: [log in to unmask] at ccmgw1 Date: 10/17/96 1:49 PM In our switch to a low solids no-clean, we are having problems with terminal solderability. I know from my reading that this is a problem thoughout industry. ASTM spec. #B545-92 gives excellent criteria for different classes. Ours being class three, we spedify the base material, a barrier layer; 50microinches of nickle and final plating; 320 microinches of tin or tin/lead(12%max lead). Terminals thus far with this specification have performed great. However, previous designed terminals have only required the terminal to be solderable. We are having a difficult time finding suppliers who will sign-up to the solderablity specification(dip test). We were lucky for many years because we used a strong OA flux, and were able to solder terminals that were substandard. We are an automotive supplier and the terminals in question are individual terminals autoinserted into boards or terminals that are part of a connector. My questions: --Is anyone else having this problem and how are you handling it? --I have heard that there are some changes being made to the J-standards specific to terminal solderablity --Does anyone have any suggestions? Thanks for your assistance Ed Holton Sr. Manufacturing Engineer [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************