Use a selective coating type system. They cost the most to implement, but have the lowest operating cost. Switching from dip to selective coat will save our plant significant money, based upon reduced coating consumption and reduced maintenance. ______________________________ Reply Separator _________________________________ Subject: ASSY:equipments for conformal coating Author: [log in to unmask] at internet Date: 10/4/96 4:48 PM Date : 4/10/96 10:23 Msg From: ATUL RASTOGI Hello,Technetters, We are going to set up a line for Automotive electronics manufacturing.There is a requirement of conformal coating on these electronics. Can someone guide us regarding the sources of the conformal coating equipment suitable for Silicone type of conformal coating using Dip or Spray method of application. Thanks in advance. Atul Rastogi Altos India Ltd Altos India Ltd *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************