Ron, Could your student be asking about Entek? If so, this is an Organic Solder Preservative manufactured by Enthone-OMI, Inc, New Haven CT (Ph 203/934-8611), marketed under the trade name ENTEK PLUS. ---------- From: TechNet-request To: rgedney Cc: technet Subject: Re: Entech Date: Thursday, October 03, 1996 11:12AM > One of our students is looking for information on the Entech coating process > for copper lines. Can anyone tell me where to find that? I have heard of it > as a process ... is it a company as well? > Ron Gedney IBM (at Wangaratta, Victoria AUSTRALIA) seem to like using it. When we were getting them to make procure & load some boards (for my old company) they insisted on it for surface flatness, shelf life & ease of soldering. Maybe they can help you if you cant find who "Entech" is. dom -- Regards, (A4fonHPUX9.0onHP715,CCTv5.2.5) JNA Telecommunications Limited ___ _____ 16 Smith Street Dom Bragge (VK2YAK) __ / / |/ / _ | Chatswood NSW 2067 PWB Designer, (R&Ddiv) / // / / __ | AUSTRALIA Tel: (+61 2) 9935 5792 \___/_/|_/_/ |_| email [log in to unmask] Fax: (+61 2) 9417 3862 http://www.jna.com.au *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************