To: Bill Kasprzak Moog Inc. A few years ago we used a "saddle", made from a plastic channel we obtained from Richco Plastic in Chicago. The plastic was Dupont FE2400 and the latest phone number I have for Richco Plastic is (312) 539-4060. Neither the saddle or the "V" standoff quite makes .060"; they are more like .035"-.040". Bruce Smith [log in to unmask] Smiths Industries Grand Rapids, MI (616) 241-8379 ______________________________ Forward Header __________________________________ Subject: Soldering CK06 Capacitors Author: [log in to unmask] at SMTPpost Date: 9/30/96 3:26 PM We are currently working a job that uses NASA spec NHB5300.4(3A-2) as a guide for Requirements for Soldered Electrical Connections. Does anyone have any tricks for supporting the body of CK06 style leaded components which are mounted radially that needs to be supported approx. .060" up off the board ??? The "S" level component is not available with the "V" standoff on the body. Thanks Bill Kasprzak Moog Inc. 716-652-2000 ext. 2507 *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** Received: from esseye.si.com by smtpgwy.si.com (SMTPLINK V2.11) ; Mon, 30 Sep 96 15:26:13 EST Return-Path: <[log in to unmask]> Received: by esseye.si.com via rmail with stdio id <[log in to unmask]> for [log in to unmask]; Mon, 30 Sep 1996 15:18:11 -0400 (EDT) (Smail-3.2 1996-Jul-4 #4 built 1996-Aug-27) Received: from simon.ipc.org by relay4.UU.NET with SMTP (peer crosschecked as: IPC.ORG [168.113.24.64]) id QQbjlc05003; Mon, 30 Sep 1996 15:10:11 -0400 (EDT) Received: from ipc.org by simon.ipc.org via SMTP (940816.SGI.8.6.9/940406.SGI) id NAA15964; Mon, 30 Sep 1996 13:50:22 -0700 Resent-Date: Mon, 30 Sep 1996 13:50:22 -0700 Received: by ipc.org (Smail3.1.28.1 #2) id m0v7mHy-0000TLC; Mon, 30 Sep 96 12:37 CDT Resent-Sender: [log in to unmask] Old-Return-Path: <[log in to unmask]> From: "Kasprzak, Bill (esd) US" <[log in to unmask]> To: IPC-Tech Net <[log in to unmask]> Subject: Soldering CK06 Capacitors Date: Mon, 30 Sep 96 13:46:00 PDT Message-Id: <[log in to unmask]> Encoding: 13 TEXT X-Mailer: Microsoft Mail V3.0 Resent-Message-ID: <"z4urq3.0.S1K.bL0Ko"@ipc> Resent-From: [log in to unmask] X-Mailing-List: <[log in to unmask]> archive/latest/6568 X-Loop: [log in to unmask] Precedence: list Resent-Sender: [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************