Scott I cannot answer your question about the Enteck and the tarnishing, but I am wondering why you have selective gold plating and the Enteck process. The electroless gold plating can be used to ensure solderability of SMT pads. We presently populate and reflow a PCB that is electroless gold over electroless nickle. The gold plate ensures the solderability of the nickle and the thickness of the gold plate is such that you do not have a gold embrittled joint.. We have been running this in production for well over a year with no solderability problems. This process was chosen because we needed a nickle pad on the PCB that contacted a nickle terminal within the housing(like metals) for wear purposes. Originally the PCB was going to be the nickle plate with HASL and the one pad would be masked off so it would stay nickle. The bare board fabrication cost was less by using the nickle plate and then the gold plate. The other process was lengthier and required masking of the one pad during the HASL step and then removal of the mask. Since gold is a noble metal, we can leave it on the contact pad with no problems and the gold ensures the solderability of the nickle. To re-ask my question--Why have a PCB with some pads gold plated and the other Enteck, thus requiring more steps in the PCB fabrication when you could have the entire PCB electroless gold plated and still have proper solderability. ------------- Original Text From: C=US/A=INTERNET/DDA=ID/TechNet-request(a)ipc.ipc.org, on 9/18/96 7:30 AM: From: Scott Westheimer Date: 9/17/96 Sorry if my message of last night was not very clear, but what can you expect at 2:30 am. The issue is with entek coating not the gold plating. The panels have selective gold plating on some pads and the others have entek. The problem is that when the panels are first gold plated( electrolydicly ), then S/M the entek pads are fine. However, when the panels are first S/M and then gold plated the entek pads are tarnished around the edges. Does anyone have experience with this problem. Thanks, PS Before anyone makes the comment, the boards are enticed after all the processes have been completed. *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************