Poh Kong Hui You stated that you are stencil printing your smd adhesive. I am aware of the process and read about it. We presently build mixed technology boards so this process is not necessary for us, we dispense adhesive because the thru-hole parts are already in the PCB. I would like to know why you chose this process, how you are using it in production and the problems and successes that you have with the process, especially in the print life and cleaning. Anyone else is welcome to answer also. Thanks Ed Holton [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text. * ***************************************************************************