.0003 min./.0015 max. ______________________________ Reply Separator _________________________________ Subject: Minimum Solder Thickness @ Assembly Author: [log in to unmask] at Internet Date: 11/21/95 9:55 AM As fabricators, we have had it drilled into us that "flat solder is best" for assembly. We have never received a return from any customer for "thin solder", but I can't say the opposite is true. My process engineers desire to alter our hot air solder leveling parameters to eliminate any future chances of returns for thick solder. Our SPC data suggests that lowering the peak solder thicknesses results in exceptionally thin solder (IMO) on certain pad geometries. My question: How thin is too thin? As assemblers, when (at what thickness or process conditions) would you return boards to the fabricator? [log in to unmask] (Glynn Shaw)