Mr. Ahlert, Can you say what your cleaning process entailed, specifically the cleaning media. Sometimes, if the media is caustic, such as a high pH saponifier, the surfaces can become unsolderable. If you would like to discuss it, you can give me a call at 317-457-8095. Doug Pauls [log in to unmask] or Terry Munson [log in to unmask]