get in touch with Hal Brown @ Zycon Corporation @ 408.241.9900 ______________________________ Reply Separator _________________________________ Subject: Double Treated Copper vs. Standard (Not Black) Oxide(s) Author: [log in to unmask] at corp Date: 11/13/95 12:45 PM Does anybody out there have (or know of) any technical reports or articles that reference peel strengths on polyimide of double treat vs. standard (reduced, brown, converted, white (tin) or red) oxide?? I know that the double treated copper has a topology that produces a more desirable adhesion/bond interface. Thanks in advance for any and all responses. Hadco Printed Circuits Tech Center Two / Watsonville _/_/_/_/_/_/_/ _/_/_/_/ _/_/_/_/_/_/ _/_/_/_/_/_/ _/_/ _/ _/_/ _/_/ _/_/ _/ _/_/ _/_/ _/_/ _/_/_/_/ _/_/_/_/_/_/ _/_/_/_/_/_/ Dave Hoover (408) 728-6677 Senior Process Engineer (408) 728-1728 Fax [log in to unmask]