Does anybody has recommendations of how should the equipment (tank design & filter system) be best set up to run electroless Ni process? Is stainless steel tank with anodic protection the best choice? What should be the best material for filter pump? Should filter cartridges or filter bag be used? What about the temperature control? And how to deal with excessive water loss as the bath is operating at high temperature (~90 deg C)? Also, what about the control of the bath constituents? Should an automatic controller be employed? How frequent should be the replenishments? Is there ever a need to dump the bath if the orthophosphite level in the bath can always be maintained at an acceptable level? What other variables are indicative of bath age besides orthophosphite content? Will really appreciate if anybody can help me answer the above questions. Thanks in advance!